MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Henkel Loctite® ABLESTIK ABP 8910T Adhesive
Categories: Polymer; Adhesive

Material Notes: Appearance: B lue

Cure: Heat cure

Product Benefits:

  • High MRT performance
  • High thermal conductivity
  • Electrically Insulating
  • High reliability
Application: Die attach

Key Substrates: Copper, Silver, PPF and Alloy 42

Filler Type: Alumina

LOCTITE ABLESTIK ABP 8910T die attach adhesive is formulated with a medium modulus using hybrid chemistry and is targeted for use on medium to large die sizes.

Information provided by Loctite®

Vendors:
Available Properties
  • Brookfield Viscosity, Uncured, CP51, Speed 5 rpm
  • Tensile Modulus, Cured, DMTA
  • Tensile Modulus, Cured, DMTA
  • Tensile Modulus, Cured, DMTA
  • Tensile Modulus, Cured, DMTA
  • Tensile Modulus, Cured, DMTA
  • CTE, linear, Cured, Below Tg
  • CTE, linear, Cured, Above Tg
  • Thermal Conductivity, Cured
  • Glass Transition Temp, Tg, Cured, TMA penetration mode
  • Cure Time, ramp to 175°C + 15 minutes @ 175°C
  • Working Life
  • Shelf Life, Uncured, from date of manufacture
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.