MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
SABIC PPE reactive chemistries SA110A
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: NORYLâ„¢ SA110A resin is a low molecular weight polymer based on polyphenylene ether (PPE). Miscibility of NORYL SA110A resin in polystyrene may allow use as a styrene endblock reinforcing resin in a variety of materials like styrene-based rubbers and styrene block copolymers. Adding NORYL SA110A resin to these systems may improve heat resistance (adhesion at elevated temperatures) while maintaining peel strength. The viscosity profile of NORYL SA110A resin makes it a good potential candidate for melt extrusion tape processes.

Information provided by SABIC

Vendors:
Available Properties
  • Viscosity, SABIC method, melt
  • Viscosity, SABIC method, melt
  • Viscosity, SABIC method, melt
  • Molecular Weight, SABIC method
  • Molecular Weight, SABIC method
  • Glass Transition Temp, Tg, SABIC method, half width
  • Gardner Color Number, ASTM D6166, 20% in Toluene, Aged 177C, 24 hrs, nitrogen
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.