This colorless liquid has a sweet, ether-like odor. It has low volatility and high boiling point. It is completely water soluble and used to produce diethylene glycol butyl acetate. Applications: Paint, Printing ink, Detergent, Coupling agent, Brake fluid, etc. Information provided by Lotte Advanced Materials. |