MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Lupolen UHM 5000 Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Lupolen UHM 5000 is an ultra high molecular weight polyethylene (UHMW PE) with an average molecular weight of 5 million. The long molecular chains lead to these properties: Highest abrasion resistance of any thermoplastic materials, excellent impact strength, low friction, good chemical resistance and stress crack resistance. Lupolen UHM 5000 is used in compression molding and ram extrusion processes. The material is supplied in form of coarse natural powder. The larger particle size and the very low fines content result in good free flowing property and less dust generation during handling and processing. Applications: Industrial, Panels & Profiles

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Bulk Density, ISO 60
  • Density, ISO 1183-1
  • Particle Size, LYB Method
  • Viscosity Test, ISO 1628-3, Intrinsic
  • Viscosity Test, ISO 1628-3, Number
  • Hardness, Shore D, ISO 868
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527-1,-2, 50mm/min
  • Tensile Strength, Yield, ISO 527-1,-2, 50mm/min
  • Tensile Modulus, ISO 527-1,-2
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179-1/1eA, double notche according to ISO 11542-2 annex B
  • Tensile Creep Modulus, 1 hour, ISO 899-1
  • Tensile Creep Modulus, 1000 hours, ISO 899-1
  • Abrasion, ISO 15527, Annex B, Abrasion Resistance (%) after 48 hours at 23°C (tool)
  • Melting Point, DSC
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75B-1,-2, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75A-1,-2, unannealed
  • Vicat Softening Point, ISO 306, B50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.