MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Morgan Advanced Ceramics Kaowool® Welt Felt ZR Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Kaowool Wet Felt and Kaowool Wet Felt ZR are manufactured from Cerablanket® and Cerachem® Blanket, respectively, which has been soaked in a specially formulated rigidizing solution that causes the blanket to harden when exposed to ambient air and/or heat. They are a “hot face” refractory insulation barrier that are designed for direct exposure to process atmospheres and can be fitted to a variety of surface contours. When dried or fired, they become a lightweight resilient insulator which can be sawed, cut, or sanded. Kaowool Wet Felt and Kaowool Wet Felt ZR are highly efficient insulators. The longer fibers give them the high tensile strength and resiliency to withstand vibration and physical abuse. Kaowool Wet Felt and Kaowool Wet Felt ZR have low thermal conductivity, low heat storage, and are extremely resistant to thermal shock.

Applications:

  • Line troughs and areas contacted with molten aluminum
  • Interior of dryers
  • Curved areas in ovens
  • Insulation for pipe wrap

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density
  • Modulus of Rupture
  • Thermal Conductivity, ASTM C201, at 15pcf
  • Thermal Conductivity, ASTM C201, at 15pcf
  • Thermal Conductivity, ASTM C201, at 15pcf
  • Melting Point
  • Maximum Service Temperature, Air, Continuous Use
  • Al2O3, after firing
  • Fe2O3, after firing
  • SiO2, after firing
  • TiO2, after firing
  • ZrO2, after firing
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.