GA-11 anatase type tio2 provides high purity, great whiteness, fine particles size, highly decoloration and strong refractive index which can bring better whiteness and opacity. With heat resistant property, GA-11 is recommended to apply to high temperature manufacturing process, such as ceramics, bricks, tiles, enamels, coatings, refractories..etc. Advantages: - High purity
- Great whiteness
- Higher brightness
- With Self-clean property
- High refractive index
- Heat resistant
Applications: - Heat resistant Ceramics
- Enamel
- Bricks, tiles
- Road paints and related paint industry
- General paint, plastic coating , rubber production
- Glass
- Comprehensive Industrial applications (paper, fiber, textile, laminate. etc.)
Information provided by Go Yen Chemical |