Temper: As Continuous Cast Casting Characteristics: High – Drossing, Shrinkage in Solidification; Medium – Fluidity, Gassing; Low - Casting Yield, Effect of Section Size Fabrication Properties: Excellent Suitability – Gas Shielded Arc Welding; Good Suitability – Soldering, Brazing, Coated Metal Arc Welding Typical uses: Safety Tools; Nuts; Stator Clamps; Bushings; Gears; Hot Mill Guides; Impellers; Pickling Equipment; Propellers; Pump Casings; Stator Clamp Segments; Valves; Wear Plates; Welding Rods; Worms; Marine Hardware Applicable Specifications: As Continuous Cast – ASTM B505/B505M; As Sand Cast – Castings ASTM B148; Ingot – ASTM B30 |