MasterSil Primer 718 is a specially formulated silicone primer for use with MasterSil RTV silicone elastomers and sealants to promote adhesion to various difficult-to-bond substrates such as acrylics, ABS, polycarbonates, polyphenylene oxides, polysulfones, polyesters, styrenics, rigid PVC’s, etc. It is a one component, low viscosity colorless liquid. |