Vinnolit® EP 6953 G PVC for paste application. Vinnolit® EP 6953 G is a medium molecular weight paste-making emulsion homopolymer, giving low viscosity plastisols. Plastisols made with Vinnolit® EP 6953 G gave a nearly Newtonian flow property. Main applications are compact and chemically blown foam formulations. Application fields are plastisols with low content of plasticizer for floor coverings, artificial leather as well as plastisols for cap closures. It is characterized by the following properties: very low initial viscosity, high viscosity stability, good thermo stability with many stabilizers, decreasing of dilatancy by proportionally, use of Vinnolit® EP 6953 G, good filler tolerance.Information provided by Vinnolit. |