MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Melos Mecoline S RDX 1215 F Halogen-free, radiation cross-linkable, flame retardant sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, radiation cross-linkable, flame retardant sheathing compound for power and telecommunication cables

Compound class: Sheathing

Compound category: RDX

Flame retardant: ATH

Standards: EN 50264 EM101-104; IEC 60092-360 SHF2; NEK 606

Typical applications: Halogen-free, low smoke, flexible at low temperatures, highly oil and extra fuel resistant, radiation cross-linkable, flame retardant compound for Offshore/Shipboard and Marine/Aerospace applications.

Features: Flame retardant; Halogen-free; Low smoke; High temperature resistant; Oil resistant; Flexible; Flexible at low temperatures

Information provided by Melos

Vendors:
Available Properties
  • Density, DIN EN ISO 1183-1A, pressed plaques, 165°C / 5 min.
  • Melt Flow, DIN EN ISO 1133
  • Hardness, Shore A, DIN ISO 7619-1, pressed plaques, 165°C / 5 min.
  • Hardness, Shore A, DIN ISO 7619-1, cross-linked plaques or tapes, 100kGy
  • Tensile Strength, IEC 60811-501, extruded tapes
  • Tensile Strength, IEC 60811-501, cross-linked plaques or tapes, 100kGy
  • Tensile Strength, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 903
  • Tensile Strength, IEC 60811-404, cross-linked plaques / tapes, EDC 95-11
  • Tensile Strength, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 903
  • Tensile Strength, IEC 60811-404, cross-linked plaques / tapes, Carbo Sea (oil based)
  • Tensile Strength, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-401, cross-linked plaques / tapes, After ageing in air oven
  • Tensile Strength, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 902
  • Elongation at Break, IEC 60811-501, cross-linked plaques or tapes, 100kGy
  • Elongation at Break, IEC 60811-501, extruded tapes
  • Elongation at Break, IEC 60811-507, Hot set test, Residual, 0.2 Mpa
  • Elongation at Break, IEC 60811-507, Hot set test, under load, 0.2 Mpa
  • Elongation at Break, IEC 60811-404, cross-linked plaques / tapes, EDC 95-11
  • Elongation at Break, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 903
  • Elongation at Break, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 903
  • Elongation at Break, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 902
  • Elongation at Break, IEC 60811-404, cross-linked plaques / tapes, Carbo Sea (oil based)
  • Elongation at Break, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 902
  • Elongation at Break, IEC 60811-401, cross-linked plaques / tapes, After ageing in air oven
  • Elongation at Break, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 902
  • Elongation at Break, IEC 60811-404, cross-linked plaques / tapes, Fluid IRM 902
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Brittleness Temperature, ASTM D 746-14, 100
  • Processing Temperature, Maximum mass temperature
  • Processing Temperature, Tool
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Zone 5
  • Adapter Temperature
  • Head Temperature
  • Drying Temperature
  • Dry Time
  • Shelf Life
  • Loss on Ignition(%), ASTM D 2863 A
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.