MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Morgan Advanced Ceramics Kaowool Millboard 1401 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: RCF Fiber Class. Kaowool Millboard products are processed from a slurry consisting of Kaowool ceramic fibers, fillers and binders. The fiber raw material is kaolin, a naturally occurring high-purity alumina-silica fireclay. Kaowool Millboard products are strong, thin, durable ceramic fiber based boards having a variety of high-temperature applications. Although these products were formulated and designed to replace asbestos millboard, their potential use extends into more conventional refractory fiber applications. Their use should be considered whenever there is a need for a thin, durable board with excellent insulating characteristics. Kaowool 1401 Millboard is a strong, thin, dense board product with excellent compression resistance and insulating characteristics. It is produced from Kaowool ceramic fibers, clay, inert fillers, and a small amount of both organic and inorganic binders for increased handling strength. It maintains its integrity throughout a wide temperature range and is easily fabricated and die cut.

Applications:

  • High-temperature gaskets (all grades)
  • Thermal barrier (grades 822 and 1401)
  • Backup insulation (grades 822 and 1401) Heat and flame shields (grade 1401)
  • Parting media (grade 1401)

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density
  • Loss On Ignition
  • Compressive Strength, at 5% deformation
  • Compressive Strength, at 10% deformation
  • Compressive Strength, at 15% deformation
  • Thermal Conductivity, ASTM C201
  • Thermal Conductivity, ASTM C201
  • Thermal Conductivity, ASTM C201
  • Thermal Conductivity, ASTM C201
  • Melting Point
  • Maximum Service Temperature, Air, Continuous Use
  • Al2O3
  • Other
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.