MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
NOVA Chemicals NOVAPOL® LA-0219-A LDPE Foam Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes:

Homopolymer

Features:

  • Versatile multipurpose foam processing
  • Good foam-processing window
  • Suitable drawdown characteristics
  • Maintains foam dimensional stability
  • Achieves packaging-foam density

Additives:

  • Base resin

Applications:

  • Edge protection
  • Foam sheet and profile extrusion
  • Conventional and cross-linked foams
  • Specialty foams

Film properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are dependent upon operating conditions.

United States: NOVAPOL LA-0219-A resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.1, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors:
Available Properties
  • Density, ASTM D 792
  • Thickness
  • Melt Flow, Melt Strength
  • Melt Index of Compound, ASTM D 1238
  • Film Tensile Strength at Yield, MD, ASTM D 882
  • Film Tensile Strength at Yield, TD, ASTM D 882
  • Tensile Strength, Yield, ASTM D 638
  • Film Elongation at Break, MD, ASTM D 882
  • Film Elongation at Break, TD, ASTM D 882
  • Elongation at Break, ASTM D 638
  • Flexural Modulus, 1% Secant, ASTM D 790
  • Coefficient of Friction, ASTM D 1894
  • Elmendorf Tear Strength MD, ASTM D 1922
  • Elmendorf Tear Strength TD, ASTM D 1922
  • Dart Drop Test, ASTM D 1709/A, F50
  • Film Tensile Strength at Break, MD, ASTM D 882
  • Film Tensile Strength at Break, TD, ASTM D 882
  • 1% Secant Modulus, MD, ASTM D 882
  • 1% Secant Modulus, TD, ASTM D 882
  • Haze, ASTM D 1003
  • Gloss, ASTM D 2457, @ 45°
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.