MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Morgan Advanced Ceramics Kaowool Mastic / Mastic F Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Mastic is a mouldable form of KaowoolTM Ceramic Fibre which can be trowelled, hand moulded, or injected from a hand-held pressure gun. Drying converts the Mastic into a strong, hard - yet light weight - insulating material which has great thermal stability up to 1000°C and can be used in some applications up to 1260°C. Resistance to cracking and spalling is excellent, and the dried material has strong adhesive properties. Although air drying is possible, it is recommended that assisted drying be carried out below 100°C. Care must be taken to ensure that the moisture can readily escape. Mastic remains stable when stored in its resealable container, and a shelf life of at least six months may be expected; however, precautions should be taken against freezing.

Typical applications: As a general stand-by repair medium for patching,sealing and caulking in furnaces, boilers etc. Also for the lining and repair of launders, ladles, casting heads and distributors for non-ferrous metals and the filling of cuplocks used on anchors in high temperature furnace linings.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density, dried
  • Density, as supplied
  • Loss On Ignition
  • Modulus of Rupture, dried
  • Modulus of Rupture, after 24 hours
  • Maximum Service Temperature, Air
  • Shrinkage, ASTM C356, isothermal heating at classification temp
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.