MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Lord Adhesives 850 Toughened Structural Acrylic Adhesive with Lord Accelerator 25GB Adhesive System
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: LORD® 850 and 852 acrylic adhesives in combination with LORD Accelerator 25GB can be used to replace welding, brazing, riveting and other mechanical fastening methods. These toughened structural adhesives perform particularly well in low-temperature environments and applications that are subject to high impact, high peel loads or high fatigue. LORD 850 and 852 adhesives provide a range of working times to accommodate a wide variety of process requirements. LORD 850 and 852 adhesives, when mixed with LORD Accelerator 25GB, create adhesive systems that bond a wide variety of prepared or unprepared metals and some engineered plastics. These adhesive systems are specifically formulated to provide the highest impact and peel strengths available in a room temperature curing adhesive with exceptional cohesive failure mode. LORD Accelerator 25GB allows precise control of the adhesive bondline thickness due to its content of glass beads.

Features: bonds a wide range of unprepared metals with minimal substrate preparation, as well as polymer composite substrates such as FRP. provides high strength for high-end structural bonding applications; 100% elongation improves impact strength and fatigue resistance. performs at temperatures from -40°F to +300°F (-40°C to +149°C); tolerates e-coat bake with cohesive failure at 338°F (170°C). resists dilute acids, alkalis, solvents, greases, oils, moisture, salt spray and weathering; provides excellent resistance to indirect UV exposure. remains in position when applied on vertical or overhead surfaces, allowing for greater process flexibility.

All information provided by Lord.

Vendors:
Available Properties
  • Density
  • Solids Content, mixed with recommended accelerator
  • Brookfield Viscosity
  • Hardness, Shore D, Cured with accelerator
  • Tensile Strength at Break, ASTM D 638, modified, Cured with accelerator
  • Elongation at Break, ASTM D 638, modified, Cured with accelerator
  • Modulus of Elasticity, ASTM D 638, modified, Cured with accelerator
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, ASTM E1640-99, by DMA, Cured with accelerator
  • Flash Point
  • Cure Time, Adhesive mixed with Accelerator, reaches 90% of its full strength after 1 hour
  • Pot Life, Time to Handling Strength, Mixed with recommended Accelerator
  • Working Life, Mixed with recommended Accelerator
  • Shelf Life, in original, unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.