MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Sandvik Bioline 4C27A Precision Wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Sandvik Bioline 4C27A is a hardenable stainless chromium steel characterized by:
  • very good machinability
  • high wear resistance
  • good toughness
  • good corrosion resistance due to addition of molybdenum
  • Sandvik Bioline 4C27A is suitable for the manufacture of precision components like watch parts, measuring points, dental tools, precision instruments and drilled surgical needles. It is also used within the automotive industry for critical applications.

    Service temperature -50 to +100°C.

    Prolonged service at elevated temperatures causes loss of corrosion resistance and hardness when used in the hardened and tempered condition.

    Information provided by Sandvik

    ASTM 420F

    Vendors:
    Available Properties
    • Density
    • Hardness, Vickers, HV5, 600°C-tempering temperature
    • Hardness, Vickers, HV5, 100°C-tempering temperature
    • Tensile Strength, Ultimate, annealed or annealed/ground, straight
    • Tensile Strength, Ultimate, annealed, coiled
    • Tensile Strength, Ultimate, drawn/ground or annealed/ground , straight
    • Tensile Strength, Ultimate, drawn or drawn/ground, straight
    • Tensile Strength, Ultimate, drawn, coiled
    • Tensile Strength, Yield, d=0.45-3mm, annealed, coiled; d=3-10mm, annealed or annealed/ground, straight
    • Tensile Strength, Yield, d=0.45-4mm, drawn, coiled; d=0.6-5mm, drawn or drawn/ground, straight
    • Tensile Strength, Yield, drawn/ground or annealed/ground , straight
    • Elongation at Break, drawn, coiled
    • Elongation at Break, drawn or drawn/ground, straight
    • Elongation at Break, drawn/ground or annealed/ground , straight
    • Elongation at Break, annealed or annealed/ground, straight
    • Elongation at Break, annealed, coiled
    • Charpy Impact, 100°C tempering temperature
    • Charpy Impact, 400°C tempering temperature
    • Charpy Impact, 600°C-tempering temperature
    • Electrical Resistivity, cold drawn
    • Electrical Resistivity, heat treated
    • CTE, linear, cold drawn
    • CTE, linear, heat treated
    • CTE, linear
    • CTE, linear
    • CTE, linear, cold drawn or heat treated
    • Maximum Service Temperature, Air
    • Minimum Service Temperature, Air
    • Carbon, C
    • Chromium, Cr
    • Iron, Fe, As Balance
    • Manganese, Mn
    • Molybdenum, Mo
    • Nickel, Ni
    • Phosphorus, P
    • Silicon, Si
    • Sulfur, S
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.