Exxtra™ Soft EMA5024 an ethylene methyl acrylate copolymer that can be used in specialty bonding applications and as a toughener for engineering polymers. It can be processed at temperatures as low as 200°F (93°C) and as high as 600°F (315°C). Availability: Latin America; North America Additive: Antiblock: No; Slip: No; Thermal Stabilizer: Yes Applications: Compatibilizer; Engineering Polymer Toughener; Low Temperature Sealant Compounds; Masterbatch Base Resin Information provided by ExxonMobil. |