MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Abhar Polymer Compounds APJAC4 Compound for Jacketing
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: APJAC4 is a black linear low density compound for jacketing of power and communication cables. APJAC4 is characterized by:
  • High melting temperature
  • Good petroleum-jelly resistance
  • Low water permeability
The excellent properties of APJAC4 will give advantages in manufacturing, installation and performance of power and communication cables. APJAC4 contains 2.5% well-dispersed (max 2 accordance BS 2782, ISO 18553) carbon black in order to ensure excellent weathering resistant.

Specifications: APJAC4 meets the applicable requirements: ASTM D1248 Type 2, Class C, Category 4, Grade J3,E5 IEC60502-ST7

Information provided by Abhar Polymer Compounds

Vendors:
Available Properties
  • Density, ASTM D792
  • ESCR 10% Igepal®, ASTM D1693
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638, after 240 hrs at 110°C
  • Elongation at Break, ASTM D638
  • Volume Resistivity, IEC60093
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, EC60243
  • Dissipation Factor, ASTM D150
  • Brittleness Temperature, ASTM D746
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Die Temperature
  • Head Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.