MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Carlson C 800AT Nickel-Iron-Chromium Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: General Description

Carlson Alloy C 800AT is a modification of Carlson Alloy C 800, exhibiting higher creep and rupture strengths. This nickel-iron-chromium alloy has a carbon content restricted to a range of 0.06 to 0.10%. The aluminum plus titanium content of this alloy is also maintained in the upper portion of the standard range (0.85 to 1.20%).

C 800AT is solution-annealed at 2100°F (1500°C). That heat treatment and the compositional restrictions are responsible for this alloy’s improved creep and rupture strengths.

Since the chemistry of C 800AT falls within the range of C 800, there are no significant differences in physical and thermal properties. The major differences between the alloys are in the mechanical properties. (Generally C 800 exhibits higher mechanical properties at room temperature and during short-term exposure to elevated temperatures.) C 800AT displays superior and rupture strengths over long-term exposure to elevated temperatures.

C 800AT offers higher ASME boiler and pressure vessel design stress allowables in creep and rupture test ranges than C 800H.

Applications

  • Chemical and Petrochemical – piping, tubing, pigtails and outlet manifolds in steam/hydrocarbon reforming; tubing for ethylene production; tubing and heaters for oxo-alcohol production; hydrodealkylation units; tubing, flanges and bends for production of vinyl chloride monomer.
  • Thermal Processing – tubing, muffles, retorts and fixtures in heat treating furnaces.
  • Power Generation – tubing in power plant superheaters and reheaters.

Information provided by Carlson

Key Words: UNS N08811
Vendors:
Available Properties
  • Density
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus, Calculated
  • Magnetic Permeability, 200 Oersted
  • Curie Temperature
  • CTE, linear
  • Melting Point
  • Solidus
  • Liquidus
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.