MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
ChevronTexaco ISO 22 Form Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Form Oil is a high quality, lightly compounded lubricant which will do an excellent job as a concrete form oil where customers desire a quick clean break from the forms.

Chevron Form Oil is a light colored oil manufactured using specially refined base oils. These base oils possess excellent natural low pour points, good "metal wetting" characteristics, and good natural film strength.

Chevron Form Oil contains an oiliness additive that improves film strength under boundary lubrication.

Applications

Chevron Form Oil is an excellent concrete form wetting agent. It can be used on any form where a release agent is recommended. Chevron Form Oil is especially recommended for the manufacture of precast concrete structures, concrete pipe, and precast concrete curbs and beams.

Chevron Form Oil, with the oiliness additive, does an excellent job in aluminum polishing.

Chevron Form Oil is recommended for use by the steel industry as a rust preventive on sheet and plate steel, wire, and cold drawn bar stock in warehouse storage.

Key Words: CPS Number: 242011; MSDS Number: 4734
Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.