LNP THERMOCOMP EC004EXAR1 compound is based on Polyetherimide (PEI) resin containing 20% carbon fiber designed to provide a Wider Process Window and Easier Flow for Large Format Additive Manufacturing (LFAM) applications needing High heat performance. PEI compounds, based on SABIC's inherently flame-retardant ULTEM™ resins, provide Low Thermal Expansion, High Temperature Performance, Excellent Strength-to-Weight Ratio, High Modulus and Low Creep. Features: High Stiffness,Low Creep Sensitivity,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant Information provided by SABIC |