MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Röhm ACRYLITE® 16 mm Resist High Impact Acrylic Double-Skin Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: 16 mm ACRYLITER Resist high impact acrylic double-skin sheet is a light transmitting, heat-insulating and weatherresistant sheet made of impact-modified acrylic (polymethyl methacrylate, PMMA) polymer. 16 mm ACRYLITER Resist high impact acrylic double-skin sheet is suitable for sloped, curved and vertical applications including the following:
  • Canopies
  • Carports
  • Clerestory Glazing
  • Interior Walls
  • Interior Partitions
  • Lighting Panels
  • Conservatories
  • Skylights
  • Barrel Vaults
  • Facades & Cladding
  • Greenhouses
  • Pool Enclosures
  • Patio Covers
  • Sunrooms
Advantages of 16 mm ACRYLITE® Resist high impact acrylic double-skin sheet
  • Extraordinary clear sheet is UV-resistant and includes a 30-year warranty against yellowing.
  • Is coated with a completely non-toxic biologically neutral Anti Algae Application
  • Offers excellent protection against excessive amounts of UV radiation.
  • Up to 50% energy savings and minimizes CO2 emissions.
  • Hail-resistant with a 10-year guarantee for withstanding hailstones with a kinetic energy of 1 joule.
  • High light transmission in the PAR and visible spectral energy wavelengths.
  • Impact resistance during transportation, handling and installation.
  • Available in clear and a range of colors and solar tints.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors:
Available Properties
  • Thickness
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Smoke Density, ASTM D2843
  • Ignition Temperature, ASTM D1929, Autoignition
  • Transmission, Visible, Solar Cool White
  • Transmission, Visible, Bronze
  • Transmission, Visible, Light White
  • Transmission, Visible, Clear
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Röhm GmbH , former product of Evonik Corporation; Evonik Cyro

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.