MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Evonik Trogamid® T5000 Nylon 6-3  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6-3 (PA63)

Material Notes: Description: TROGAMID® T compounds are distinguished by the following properties:
  • crystal-clear, optical transparency
  • high mechanical stability
  • high thermostability
  • high viscosity
  • good chemical resistance compared to other plastics
  • good electrical properties
  • low mold shrinkage

The special properties of TROGAMID T have made it useful in many branches of industry:

  • Electrical Industry:
    • high-voltage switch casings
    • cable glands
    • battery seals
    • keys and push buttons
    • terminal strips
    • casings for switches, relays, and counters
    • gearwheels and gear racks
  • Water Resource Management and Filter Technology:
    • filter cups for pneumatic systems
    • filter cups for water treatment
    • fuel filter cups
    • pump casings
    • metering devices
    • inspection glasses
  • Machine and Apparatus Construction:
    • flowmeters
    • liquid-level indicators
    • valve blocks and common control blocks for dispensing and metering equipment
    • guide rails

Specific Notes for this Material: Permanently transparent polyamide for injection molding, extrusion, and blow molding; no additives

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA 6-3-T, PA NDT/INDT, trimethyl hexamethylene diamine terephthalic acid
Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity Number, ISO 307
  • Hardness, Shore D, ISO 868
  • Ball Indentation Hardness, ISO 2039-1, H30
  • Tensile Strength, Yield, ISO 527-1/2, 50 mm/min
  • Elongation at Break, ISO 527-1/2, 50 mm/min
  • Elongation at Yield, ISO 527-1/2, 50 mm/min
  • Elongation at Yield, ISO 178, 5 mm/min, Outer fiber strain at maximum stress
  • Tensile Modulus, ISO 527-1/2
  • Flexural Strength, ISO 178, 5 mm/min, at 3.5% Strain
  • Flexural Strength, ISO 178, 5 mm/min
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Tensile Creep Modulus, 1 hour, ISO 899-1
  • Tensile Creep Modulus, 1000 hours, ISO 899-1
  • Abrasion, DIN 53754, Abrasion Resistance, mg/100 rev.
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Surface Resistance, IEC 60093, Spec.
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1, K20/P50
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112, Test Solution A, 100 drops
  • CTE, linear, ISO 11359, Longitudinal
  • CTE, linear, Transverse to Flow, ISO 11359
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/2
  • Vicat Softening Point, ISO 306, 10N
  • Vicat Softening Point, ISO 306, 50N
  • Glass Transition Temp, Tg, Tg, 10 K/min
  • UL RTI, Mechanical with Impact, UL 746 B
  • UL RTI, Mechanical without Impact, UL 746 B
  • Flammability, UL94
  • Flammability, UL94
  • Glow Wire Test, IEC 60695-2-1/0-3
  • Transmission, Visible, transparent; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.