MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Momentive Performance Materials GE Silicones IGS3763 Two-Component Insulating Glass Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: IGS3763 adhesive silicone is an optimized, high-modulus, neutral curing sealant for edge seal applications for gas and air filled structural and non- structural insulating glass units. IGS3763 two-component silicone offers variable work life with fast deep section cure to accommodate scheduling and production needs.

Features: High Modulus, High Elastic Recovery, Fast Cure, Compatibility, Non-flammable.

Applications: Structural Glazing, Silicone Durability, Adhesive. Note: IGS3763 silicone should only be used in the fabrication of insulating glass where the dual seal method of fabrication is used. The moisture vapor transmission rate of silicone sealants is sufficiently high as to preclude their use in the fabrication of single seal insulating glass units. Silicone setting blocks are recommended for direct contact with IGS3763 silicone. Avoid using non-silicone materials (i.e., EPDM, Neoprene) as they could degrade or discolor the secondary seal over time. Avoid IGS3763 to be in contact with or exposed to sealants that evolve acetic acid cure byproduct. Not recommended for water immersion applications.

IGS3767 is the gray equivalent.

Information provided by Momentive Performance Materials.

Vendors:
Available Properties
  • Specific Gravity, Component B
  • Specific Gravity, Mixed; uncured
  • Specific Gravity, Component A
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, ISO 8339
  • Tensile Strength, ASTM C1135
  • Tensile Strength, Ultimate, ASTM D412
  • Tensile Stress at Strain, ASTM C1135
  • Tensile Stress at Strain, ISO 8339
  • Tensile Stress at Strain, ASTM C1135
  • Elongation at Break, ASTM C1135
  • Elongation at Break, ISO 8339
  • Elongation, Ultimate, ASTM D412
  • Modulus of Elasticity, ETAG 002
  • Shear Strength, ASTM C961
  • Tear Strength, ASTM D624, die B
  • Maximum Service Temperature, Air, Heat Resistance
  • Tack-Free Time, 2X snap time
  • Shelf Life, Component B, when properly stored.
  • Shelf Life, Component A, when properly stored.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Momentive Performance Materials (GE Silicones)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.