MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Bearing Bronze, UNS C93700, Copper Casting Alloy, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Fabrication Properties: Good Suitability – Brazing, Soldering

Typical uses: Brackets; Nuts; Washers for Engines; Applications Requiring Acid Resistance to Sulphite Fluids; Bearing Plates; Bearings; Bushings; Bushings for high speed and heavy pressure.; Corrosion Resistant Castings; Crank Shafts; High Speed, Heavy Load Bearings; Impellers; Machine Parts; Parts for Steel Mill Maintenance; Pressure Tight Castings; Pumps; Slide Guides for Steel Mills Large Bearings for Ships

Applicable Specifications: As Centrifugal Cast – Castings SAE J461, Castings AMS 4842, Castings SAE J462, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings AMS 4842, Castings ASTM B763/B763M, Castings SAE J462, ASTM B66, Castings SAE J461, Castings ASTM B584, Castings ASME SB584, Castings ASTM B22/B22M; Bearings & Busings AMS 4827; Ingot - ASTM B30

Vendors:
Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, for Standard
  • Tensile Strength, Typical
  • Tensile Strength, Yield, for Standard, 0.5% Ext
  • Tensile Strength, Yield, 0.2% Offset
  • Tensile Strength, Yield, Typical, 0.5% Ext
  • Elongation at Break, for Standard
  • Elongation at Break, Typical
  • Creep Strength, 0.1% per 10,000 hours
  • Tensile Modulus
  • Compressive Strength, 0.001 in. set/in.
  • Compressive Strength, 0.1 in. set/in.
  • Fatigue Strength
  • Machinability
  • Shear Strength
  • Izod Impact
  • Charpy Impact, V-Notch
  • Electrical Resistivity, 10% IACS
  • Magnetic Permeability
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, Incipient
  • Melting Point
  • Solidus
  • Liquidus
  • Processing Temperature, Stress Relief
  • Aluminum, Al
  • Antimony, Sb
  • Copper, Cu
  • Iron, Fe
  • Lead, Pb
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Tin, Sn
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.