MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: TECAFORM® UD Blue is an Ultra Detectable acetal copolymer designed specifically for applications in the food industry. High speed food production lines detect particulate matter in the food product one of three ways; Using optical scanners, metal detection equipment, or X-ray equipment. TECAFORM® UD Blue is the first engineering thermoplastic that will show up regardless of the scanning method used.

Features:

  • Food contact blue in color
  • High visibility of filler
  • Detectable by X-ray or metal detection equipment
  • Plastic chunks as small as 3mm thick detected using standard metal detection equipment
  • Plastic shavings to 1mm thick detected using standard metal detection equipment
  • Easily machined

Information Provided by Ensinger, Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D790
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695, at 10% deformation
  • Compressive Modulus, ASTM D695
  • Izod Impact, Notched, ASTM D256
  • Melting Point, ASTM D3418
  • Maximum Service Temperature, Air, UL746B, Long Term
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.