Availability: Asia Pacific; Europe; North America Fillers/Reinforcement: Glass Fiber, 6% Filler by Weight Additive: Heat Stabilizer; Lubricant Features: Creep Resistant; Good Dimensional Stability; Good Stiffness; Heat Stabilized; Lubricated Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |