Features: Very resilient product with excellent resistance to abrasion and tearing, low temperature flexibility, and resistant to certain chemicals. Uses: Hot melt adhesive, synthetic leather and fabric coating Available in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |