MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Syensqo (Solvay Specialty Polymers) KetaSpire® KT-820UFP PEEK, Ultra-fine powder form of KT-820 resin
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: KetaSpire® KT-820UFP is the low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-colored, ultra-fine powder form. This ultra-fine PEEK powder is suitable for water-borne coatings, electrostatically driven powder coatings and resin pre-impregnation of continuous fiber composites. This ultra-fine powder is produced to a median particle size D50 of about 10 micrometers.

KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent chemical resistance to acids, bases and a broad range of aggressive organic chemicals, best-in-class fatigue resistance, high thermal resistance, high purity and ease of melt processing.

These properties make KT-820UFP well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses.

The resin is also available in a natural-colored pellet form under the grade name KT-820 NT for injection molding and extrusion.

Applications: Aerospace Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Oil/Gas Applications

Features: Chemical Resistant; Ductile; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; High Heat Resistance

Injection notes: Back Pressure: minimum

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Particle Size
  • Viscosity, ASTM D3835, Melt
  • Melt Flow, ASTM D1238
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • CTE, linear, Parallel to Flow, ASTM E831
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Glass Transition Temp, Tg, DSC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.