MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Epoxy Technology EPO-TEK® H62 Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Product Description: EPO-TEK® H62 is a single component, electrically insulating, and thermally conductive epoxy adhesive. It may be used for heat-sinking semiconductor, hybrids, or electronic circuits.

Advantages & Application Notes:

  • Black and opaque appearance; it can block out light in opto-electronic devices.
  • Semiconductor encapsulant for COB packaged die. It may be used as a glob top DAM around the chip.
  • SMD “staking” material or Surface Mount Adhesive (SMA). The SMA may be used for double-sided PCB bonding of components; staking caps and resistors to ceramic or hybrid circuits. High viscosity adhesive paste has enough wet “green strength” to hold SMD’s to the PCB prior to cure.
  • Alternatives are available in different viscosity ranges and colors.
  • Excellent adhesion to ferrous and non-ferrous metals, glass, ceramics, PCB, and most plastics.
  • Thixotropic paste appearance makes it capable of syringe dispensing techniques, stencil or screen printing, or hand applications by brush or spatula.

Information Provided by Epoxy Technology

Vendors:
Available Properties
  • Specific Gravity
  • Particle Size
  • Viscosity, 10 rpm
  • Ionic Impurities - Na (Sodium)
  • Ionic Impurities - K (Potassium)
  • Ionic Impurities - Cl (Chloride)
  • Hardness, Shore D
  • Tensile Modulus, Storage
  • Shear Strength, Lap
  • Shear Strength, Die
  • Volume Resistivity
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear, Below Tg
  • CTE, linear, Above Tg
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Intermittent
  • Minimum Service Temperature, Air, Continuous
  • Minimum Service Temperature, Air, Intermittent
  • Glass Transition Temp, Tg, Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
  • Decomposition Temperature, Degradation Temperature
  • Transmission, Visible
  • Cure Time, minimum
  • Cure Time, minimum
  • Pot Life
  • Shelf Life, refrigerated
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.