MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Shinil Chemical SHINCON PMMA Electro Conductive Polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's patented conductive filler dispersion technology with variety of engineering polymers and their alloys to impart permanent static dissipative to electrically conductive property to thermoplastics. SHINCON contains multiwall carbon nanotube (MWCNT), carbon black (CB), and carbon fiber (CF) as a conductive filler. SHINCON are used in injection molding, film or sheet extrusion for the applications where the desired level of conductivity and unique mechanical property are important. A wide range of the surface resistaivity is obtained by SHINCON formulations for the parts and devices depending upon customer needs and applications.

    Feature and Benefits
  • Permanent electro conductivity
  • Maintain the physical properties of base resin
  • No particulates (CNT product)
  • Lighter weight
  • Recyclability
  • Easy processing
  • Improved surface
  • Cost effective

Grade/Application: Pelicle box

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors:
Available Properties
  • Specific Gravity
  • Tensile Strength, Ultimate
  • Flexural Strength
  • Flexural Modulus
  • Izod Impact, Notched
  • Volume Resistivity
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.