MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Teknor Apex Chemlon® 225-15 MGH Nylon 6, 15/25% Glass Fiber/Mineral Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Availability: Asia Pacific; Europe; North America

Fillers/Reinforcement: Glass Fiber, 15% Filler by Weight; Mineral, 25% Filler by Weight

Features: Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Rigidity; High Strength; Low Warpage

Automotive Specifications: CHRYSLER MS-DB-41 CPN2927 Color: BK001 Black; FORD WSK-M4D822-A; GM GMP.PA6.012 Color: Natural; GM GMW8752-PA6-M25-GF15H

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Maximum Moisture Content
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Volume Resistivity, ASTM D257
  • Dielectric Strength, ASTM D149
  • Comparative Tracking Index, UL 746
  • CTE, linear, Parallel to Flow, ASTM D969
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • UL RTI, Electrical, UL 746
  • UL RTI, Electrical, UL 746
  • UL RTI, Electrical, UL 746
  • UL RTI, Mechanical with Impact, UL 746
  • UL RTI, Mechanical with Impact, UL 746
  • UL RTI, Mechanical with Impact, UL 746
  • UL RTI, Mechanical without Impact, UL 746
  • UL RTI, Mechanical without Impact, UL 746
  • UL RTI, Mechanical without Impact, UL 746
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Injection Pressure
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.