MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Foam

Material Notes: Medium grade silicon sponge. UL recognized for flame retardance and gasketing.

Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products, Seals in equipment access panels, Electrical and electronic enclosure gaskets, Solder gun insulation pads for work stations

Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568 corrosion resistance. Passes SMP-800-C & BSS toxic gas emission rating. Passes hot flex at 230°C (446°F) per ASTM D-573.

General BISCO™ silicone information: BISCO™ Cellular Silicones are used as sealing cushioning, vibration isolation, insulation, and thermal management gaskets. Their resistance to environmental extremes, mechanical resilience, and safety features lead to their use in transportation equipment, communications and electrical enclosures, electronic products and components, industrial machinery, and appliances.

Data provided by Rogers Corporation.

Vendors:
Available Properties
  • Density, ASTM D3574
  • Water Absorption, ASTM D471
  • Tensile Strength, Ultimate, ASTM D412
  • Elongation at Break, ASTM D412
  • Compressive Yield Strength, at 25% deflection; ASTM D1056
  • Compression Set, ASTM D1056
  • Compression Set, ASTM D1056
  • Electrical Resistivity, ASTM D257
  • Dielectric Constant
  • Dielectric Strength, ASTM D150
  • Arc Resistance, Dry; ASTM D495
  • Thermal Conductivity, ASTM C158
  • Maximum Service Temperature, Air, Recommended use; SAE J-2236
  • Maximum Service Temperature, Air, Intermittent; Rogers internal test
  • Minimum Service Temperature, Air, Recommended use; SAE J-2236
  • Brittleness Temperature, Low temp embrittlement; ASTM D746(B)
  • Flammability, UL94, Listed (may vary with thickness, color, density)
  • Flame Spread Index, IS; ASTM E162
  • Smoke Density, DX at 1.5 minutes; ASTM E662
  • Smoke Density, DX at 4 minutes; ASTM E662
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.