MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Kennametal Stellite Stellite® 250
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.

Applications:heat treatment furnaces, metallurgical industrial furnaces such as copper smelters, baskets, grates, tray, slab skids, reheat furnaces, gas and pulverized coal burners, discharge rolls and channels, radiant tube supports, and parts in contact with molten slags and molten copper.

Corrosion: Good resistance to oxidation by air or air SO2 mixtures, and corrosive resistance by H2S up to 1249°C (2280°F). Not corroded by molten copper, but it is attacked by molten zinc and aluminum. In aqueous media, withstands attack by dilute sulfuric acid and by boiling concentrated nitric acid, but is attacked by reducing acids such as HCl.

Machinability: Has tendency to work harden, can be machined with grade C² or C³ tungsten carbide tools. A stress relief treatment of 935°C (1650°F) for 4 hours and slow cooling will aid machining.

Data provided by the manufacturer, Deloro Stellite, Inc.

Product of former Deloro Stellite Inc. Similar alloys include Stellite 251, Stellite 238, UMCO-50/51, Haynes 150, Esco 72

Vendors:
Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Brinell
  • Hardness, Brinell
  • Hardness, Brinell
  • Hardness, Brinell
  • Hardness, Knoop, Converted from Rockwell C hardness.
  • Hardness, Rockwell A, Converted from Rockwell C
  • Hardness, Rockwell B, Converted from Rockwell C
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Charpy Impact, Charpy V-notch at RT
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co, As remainder
  • Iron, Fe
  • Manganese, Mn
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Kennametal Stellite, former Deloro Stellite Inc

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.