LNP LUBRICOMP WFL34H compound is based on Polybutylene Terephthalate (PBT) resin containing 20% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant, Healthcare. Features: Healthcare,Wear resistant Information provided by SABIC |