MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Matexcel NAT-0066 In Situ Forming Silk Fibroin Gel Kits
Categories: Wood and Natural Products

Material Notes: The in situ-forming and injectable silk hydrogel can be used as a drug and cell delivery carrier for researches in tissue engineering/repair and drug delivery. The drugs and cells to be delivered can be pre-mixed with regenerated silk fibroin solution and further mixed with other components provided in the kit to quickly form hydrogel. Silk hydrogel is distinguished from other biomaterial hydrogels by providing excellent mechanical strength, chemical and physical stability, biocompatibility and degradability.

Application: The component A provided in the kit can be quickly dissolved into solution, which transforms into hydrogel after mixing with Component B and C using syringes and an adaptor provided. The gel preparation can either be conducted on site by the users themselves (in situ-forming), with the entire manipulation less than 5 min, or the gel can be prepared and pre-packed in syringes or tubes by the manufacturer so that it can be used directly. Depending on the applications, the in-situ forming hydrogel can be prepared in a concentration range 1-30%, thus ideal for encapsulation and delivery of cells and drugs for in vitro and in vivo studies.

Morphology: Gel Kit

Key Words: Source: Degummed Bombyx mori silkworm
Vendors:
Available Properties
  • Storage Temperature, Storage in a dry, ventilated place at room temperature.
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.