MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Chevron Phillips 6109FK Linear low density polyethylene blown film resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Resin Type: linear low density polyethylene, butene copolymer, medium antiblock, medium slip, process aid version of 6109, blown film resin

Characteristics: good stiffness at thin gauges, good drawdown, can be used straight or blended with LDPE or HDPE, neutral screw condition

Applications: industrial liners, carrier bags, garment bags, coextrusions

Natural Color. 1000 ppm Slip. 5000 ppm Antiblock.

Film properties below based on thickness of 0.0318 mm. Extruder 6.35 cm. Screw L/D ratio 24:1. Die opening 0.1905 cm. Blow-Up Ratio 2:1.

Information provided by Chevron Phillips Chemical Company

Vendors:
Available Properties
  • Density, ASTM D4833-89
  • Melt Flow, ASTM D1238
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Secant Modulus, MD, ASTM D882
  • Secant Modulus, TD, ASTM D882
  • Coefficient of Friction, ASTM D1894
  • Elmendorf Tear Strength, MD, ASTM D1922, Orientation not specified
  • Elmendorf Tear Strength, TD, ASTM D1922
  • Dart Drop, ASTM D1709, F-50 at 26 in.
  • Dart Drop Test, ASTM D1709, F-50 at 26 in.
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • Haze, ASTM D2457
  • Gloss, 45°, ASTM D 2457
  • Gloss, 60°, ASTM D 2457
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chevron Phillips Chemical Company LP; ChevronPhillips

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.