MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Lord Adhesives 7545 Urethane Adhesive, 7545-F Curative Adhesive System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: LORD® 7545 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive also bonds primed metals and various combinations of dissimilar substrates. LORD 7545 adhesive system is available in a range of working times to accommodate a wide variety of process requirements. After opening, protect adhesive from excessive exposure to moisture by installing desiccant cartridges and/or using dry nitrogen as an inert cover.

Features: demonstrates high strength and excellent durability for structural applications. exceeds U.S. DOT requirements for non-flammability and does not require explosion-proof equipment. off-white color of cured adhesive provides an acceptable appearance when non-painted or visible. does not contain ozone depleting chemicals. resists sunlight, weathering, humidity and salt spray. solvent resistant when cured. Painting and most cleaning processes do not affect bond strength. remains in position when applied on vertical or overhead surfaces, allowing for greater process flexibility.

All information provided by Lord.

Vendors:
Available Properties
  • Density
  • Solids Content, by weight, mixed with curative
  • Brookfield Viscosity
  • Flash Point, closed cup
  • Pot Life, time to handling strength, mixed with resin
  • Working Life, working time, mixed with resin
  • Shelf Life, in original, unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.