MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Toray AMILAN™ CM3001G30 Nylon 66, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Reinforced, standard, PA66-GF30.

General Amilan™ Notes: AMILAN™ nylon (polyamide) is a thermoplastic engineering plastic containing an amide group (-CONH-) and it exhibits excellent strength, toughness, heat resistance, and anti-friction wear resistance. A variety of grades designed for various customer needs and applications are available.

Information provided by Toray Resin Co.

Vendors:
Available Properties
  • Density, ISO 1183, Dry
  • Water Absorption, ISO 62, In 23°C water, polymer initally dry
  • Water Absorption, ISO 62, In 23°C water, polymer initally dry
  • Linear Mold Shrinkage, Flow, Toray Method, 80x80x3mmt. Dry
  • Linear Mold Shrinkage, Transverse, Toray Method, 80x80x3mmt. Dry
  • Hardness, Rockwell M, ISO 2039-2, Dry
  • Hardness, Rockwell R, ISO 2039-2, Dry
  • Hardness, Rockwell R, ISO 2039-2, Dry
  • Tensile Strength, ISO 527-1,2, 1.9% Moisture Content
  • Tensile Strength, ISO 527-1,2, Dry
  • Tensile Strength, ISO 527-1,2, 1.5% Moisture Content
  • Tensile Strength, ISO 527-1,2, Dry
  • Tensile Strength, ISO 527-1,2, 1.5% Moisture Content
  • Tensile Strength, ISO 527-1,2, Dry
  • Elongation at Break, ISO 527-1,2, Dry
  • Elongation at Break, ISO 527-1,2, Dry
  • Elongation at Break, ISO 527-1,2, 1.5% Moisture Content
  • Elongation at Break, ISO 527-1,2, 1.5% Moisture Content
  • Elongation at Break, ISO 527-1,2, Dry
  • Elongation at Break, ISO 527-1,2, 1.5% Moisture Content
  • Flexural Strength, ISO 178, 1.5% Moisture Content
  • Flexural Strength, ISO 178, Dry
  • Flexural Strength, ISO 178, 1.5% Moisture Content
  • Flexural Strength, ISO 178, Dry
  • Flexural Strength, ISO 178, 1.5% Moisture Content
  • Flexural Strength, ISO 178, Dry
  • Flexural Modulus, ISO 178, 1.5% Moisture Content
  • Flexural Modulus, ISO 178, Dry
  • Flexural Modulus, ISO 178, 1.5% Moisture Content
  • Flexural Modulus, ISO 178, Dry
  • Flexural Modulus, ISO 178, 1.5% Moisture Content
  • Flexural Modulus, ISO 178, Dry
  • Compressive Strength, ISO 604, 1.5% Moisture Content
  • Compressive Strength, ISO 604, 1.5% Moisture Content
  • Compressive Strength, ISO 604, Dry
  • Compressive Strength, ISO 604, Dry
  • Compressive Strength, ISO 604, 1.5% Moisture Content
  • Compressive Strength, ISO 604, Dry
  • Shear Strength, ASTM D732, 1.5% Moisture Content
  • Shear Strength, ASTM D732, Dry
  • Charpy Impact Unnotched, ISO 179, Dry
  • Charpy Impact Unnotched, ISO 179, Dry
  • Charpy Impact Unnotched, ISO 179, 1.5% Moisture Content
  • Charpy Impact Unnotched, ISO 179, 1.5% Moisture Content
  • Charpy Impact, Notched, ISO 179, V-Notched. Dry
  • Charpy Impact, Notched, ISO 179, V-Notched. 1.5% Moisture Content
  • Charpy Impact, Notched, ISO 179, V-Notched. Dry
  • Charpy Impact, Notched, ISO 179, V-Notched. 1.5% Moisture Content
  • Coefficient of Friction, Suzuki Method, Vs Metal. Dry. Without lubrication
  • Taber Abrasion, mg/1000 Cycles, ISO 9352, Dry
  • Volume Resistivity, IEC 60093, 1.5% Moisture Content
  • Volume Resistivity, IEC 60093, Dry
  • Dielectric Constant, IEC 60250, 60% RH. (1.5% Moisture Content)
  • Dielectric Constant, IEC 60250, 60% RH. (1.5% Moisture Content)
  • Dielectric Constant, IEC 60250, 60% RH
  • Dielectric Constant, IEC 60250, 60% RH
  • Dielectric Constant, IEC 60250, 60% RH. (1.5% Moisture Content)
  • Dielectric Constant, IEC 60250, 60% RH. (1.5% Moisture Content)
  • Dielectric Strength, IEC 60243-1, 1.5% Moisture Content
  • Dielectric Strength, IEC 60243-1, Dry
  • Dissipation Factor, IEC 60250, 60% RH. (1.5% Moisture Content)
  • Dissipation Factor, IEC 60250, 60% RH
  • Dissipation Factor, IEC 60250, 60% RH
  • Dissipation Factor, IEC 60250, 60% RH. (1.5% Moisture Content)
  • Dissipation Factor, IEC 60250, 60% RH. (1.5% Moisture Content)
  • Dissipation Factor, IEC 60250, 60% RH. (1.5% Moisture Content)
  • Arc Resistance, UL-746A, Tungsten Electrode. Dry
  • Arc Resistance, UL-746A, Tungsten Electrode. 1.5% Moisture Content
  • CTE, linear, Parallel to Flow, ISO 11359-2, Dry
  • Specific Heat Capacity, Dry
  • Thermal Conductivity, Dry
  • Melting Point, DSC Method, Dry
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1,2, Dry
  • Flammability, UL94, 1.5% Moisture Content
  • Flammability, UL94, Dry
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.