MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Teknor Apex Sinpolene MBW0771 LLDPE Titanium Dioxide Masterbatch
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Sinpolene MBW0771 is a polyethylene-based pure white masterbatch designed specifically for use in tubular film blowing, blow molding and extrusion of polyolefins. With its high pigment loading, it offers high coloring value with excellent quality and performance. The blue undertone of this masterbatch is attributed by specialty selected high performance, fine crystal size rutile titanium dioxide. It is delivered as free flowing pellets for processing convenience.

Characteristic:

  • Easy processing
  • Good dispersion
  • Excellent whiteness
  • High opacifiying power
Availability: Asia Pacific

Filler/Reinforcement: Titanium Dioxide Equivalent, 70% Filler by Weight

Features: General Purpose

Uses: Film

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Blown Film

Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ASTM D792
  • Maximum Moisture Content, ASTM D3030
  • Melt Flow, ASTM D1238
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.