MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
General Plastics LAST-A-FOAM® EF-4003 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: LASTAFOAM ® EF4000 foams provide outstanding protection in impact and shock absorption applications. They exhibit relatively “flat” load deflection curves, absorbing energy while exposing delicate parts to consistent lower level stresses. These foams are manufactured in the density range of 3 to 7 lbs. cubic foot. This material can provide superior vibration dampening and cushioning for loads in the 0.1 to 2.0 psi static stress load range. They are available as flexible polyurethane foam sheets and blocks.
Shock Absorbing Polyurethane Foam: This extremely durable polyurethane foam series is formulated to absorb applications below 180°F. For a Flame-resistant version, specify LASTAFOAM ® EFR400x formulations. In aerospace and defense applications, EF4000 flexible foams have been used extensively as “spring damper” shock isolation systems to protect missiles in underground silos and nuclear submarine launch tubes. These products have been used extensively in the Polaris and Trident programs for padding on the closures of missile nose cones. They have also served as packaging and support pads for the Air Launch Cruise Missile (ALCM), and been used in the Minuteman and Peacekeeper programs. In construction, these flexible urethane foams serve as shock isolation systems for earthquake prone buildings. They also provide shock mounts and pads for delicate equipment in shipping containers, and vibration damper pads for mechanical equipment.

Advantages:

  • Superior vibration isolation and cushioning (0.1 to 2.0 psi static stress load range)
  • Extremely long lasting
  • Relatively unharmed by environmental factors
  • Absorbs significant energy while protecting payloads
Applications
  • Underground missile silos
  • Nuclear submarine launch tubes
  • Shock isolation systems for earthquake prone buildings
  • Shock mounts and pads for shipping delicate items
  • Vibration damper pads for mechanical equipment

Information provided by General Plastics Manufacturing Company

Vendors:
Available Properties
  • Density
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.