MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives

Unit of Measure Converter

Unit Converter
Equivalent Values
UOM Value
cable lengths 0.0000146
chains (Gunter's) 0.000158
cubits 0.00693
fathoms 0.00173
ft 0.0104
furlongs 0.0000158
hands 0.0312
in 0.125
km 0.00000317
leagues 6.34e-7
leagues (nautical) 6.34e-7
links (Gunter's) 0.0158
links (Ramden's) 0.0104
m 0.00317
microns 3170
mil 125
miles (nautical, Int.) 0.00000171
miles (statute) 0.00000197
mm 3.17
nm 3.17e+6
picas 0.752
points 9.02
rods 0.000630
spans 0.0139
varas 0.00374
yards 0.00347
 

MatWeb has also provided a reference table for converting between English and Metric units.

To Convert From: To: Multiply By:
lbf/in2 (psi) pascal (Pa) 6894.757
pascal (Pa) lbf/in2 (psi) 1.4504E-4
g/cm3 lb/ft3 62.427974
lb/ft3 kg/m3 16.01846
lb/in3 kg/m3 27,679.90
lb/ft3 g/cm3 0.01601846
volts/mil kV/mm 0.039370
mil (0.001 inch) cm 2.54E-3
cm mil 393.70
MPa(m1/2) psi(in1/2) 910.06
J/(g-°C) BTU/(lb-°F) 0.239006
BTU/(lb-°F) J/(g-°C) 4.184000
joule (J) cal (thermochemical) 0.2390057
cal (thermochemical) joule (J) 4.184000
joule (J) BTU (thermochemical) 9.4845E-4
BTU (thermochemical) joule 1054.350
µm/(m-°C) µin/(in-°F) 0.55556
µin/(in-°F) µm/(m-°C) 1.80
cm3/Kg in3/lb 0.027680
in3/lb cm3/kg 36.127
W/(m K) BTU in /(hr ft2  F) 6.9334713
BTU in /(hr ft2  F) W/(m K) 0.1441314
(J m)/(min m2  C) W/(m-K) 0.016667
W/(m-K) (J m)/(min m2  C) 60
© MatWeb:  This table may be copied, but the copyright and hyperlink to MatWeb must not be removed.
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.