MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Material Category Search

Find a Material Category:
Select a Material Category: Selected Material Category:
  Search Results
There are 62 materials in the category Nylon 12, 50% Glass Fiber Filled. If your material is not listed, please refer to our search strategy page for assistance in limiting your search.

Found 62 Results -- Page of 2 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Nylon 12, 50% Glass Fiber Filled
 2DiscontinuedALM PA 615-GF Nylon 12 SLS Prototyping Polymer, 50% Glass Filled
 3Arkema Rilsamid® AZM 50 BLACK T6LD PA12-GF50
 4Evonik VESTAMID® LC-GF50 BK Nylon 12, 50% Glass Fiber Reinforced
 5EMS-Grivory Grilamid® LBV-50H FWA black 9225 PA12-GF50
 6EMS-Grivory Grilamid® LBV-50H FWA nat PA12-GF50
 7EMS-Grivory Grilamid® LBV-65H FWA black 9225 PA12-GF65
 8EMS-Grivory Grilamid® LBV-65H FWA nat PA12-GF65
 9EMS-Grivory Grilamid® LV-50H FWA black 9225 PA12-GF50
 10EMS-Grivory Grilamid® LV-50H FWA nat PA12-GF50
 11EMS-Grivory Grilamid® LV-5H PA12-GF50
 12EMS-Grivory Grilamid® LV-65H FWA black 9225 PA12-GF65
 13EMS-Grivory Grilamid® LV-65H FWA nat PA12-GF65
 14EMS-Grivory Grilamid® LV-65H SST black 9288 PA12-GF65
 15EMS-Grivory Grilamid® LV-65H SST nat PA12-GF65
 16EMS-Grivory Grilamid® LVX-50H black 9230 PA12-GF50
 17EMS-Grivory Grilamid® LVX-50H nat PA12-GF50
 18EMS-Grivory Grilamid® LVX-65H SST black 9288 PA12-GF65
 19EMS-Grivory Grilamid® LVX-65H SST nat PA12-GF65
 20EMS-Grivory Grilamid® TRVX-50X9 black 9230 PAMACM12-GF50
 21EMS-Grivory Grilamid® TRVX-50X9 nat PAMACM12-GF50
 22DiscontinuedEMS-Grivory Grilamid® XE 3915 PA12-GF50
 23EMS-Grivory Grilamid® LBV-50H FWA black 9225 Nylon 12, 50% Glass Fiber Filled, Dry
 24EMS-Grivory Grilamid® LBV-50H FWA black 9225 Nylon 12, 50% Glass Fiber Filled, Conditioned
 25EMS-Grivory Grilamid® LBV-50H FWA nat Nylon 12, 50% Glass Fiber Filled, Dry
 26EMS-Grivory Grilamid® LBV-50H FWA nat Nylon 12, 50% Glass Fiber Filled, Conditioned
 27EMS-Grivory Grilamid® LBV-65H FWA black 9225 Nylon 12, 65% Glass Fiber Filled, Dry
 28EMS-Grivory Grilamid® LBV-65H FWA black 9225 Nylon 12, 65% Glass Fiber Filled, Conditioned
 29EMS-Grivory Grilamid® LBV-65H FWA nat Nylon 12, 65% Glass Fiber Filled, Dry
 30EMS-Grivory Grilamid® LBV-65H FWA nat Nylon 12, 65% Glass Fiber Filled, Conditioned
 31EMS-Grivory Grilamid® LV-5H Nylon 12, 50% Glass Fiber Filled, Dry
 32EMS-Grivory Grilamid® LV-5H Nylon 12, 50% Glass Fiber Filled, Conditioned
 33EMS-Grivory Grilamid® LV-50H FWA black 9225 Nylon 12, 50% Glass Fiber Filled, Dry
 34EMS-Grivory Grilamid® LV-50H FWA black 9225 Nylon 12, 50% Glass Fiber Filled, Conditioned
 35EMS-Grivory Grilamid® LV-50H FWA nat Nylon 12, 50% Glass Fiber Filled, Dry
 36EMS-Grivory Grilamid® LV-50H FWA nat Nylon 12, 50% Glass Fiber Filled, Conditioned
 37EMS-Grivory Grilamid® LV-65H FWA black 9225 Nylon 12, 65% Glass Fiber Filled, Dry
 38EMS-Grivory Grilamid® LV-65H FWA black 9225 Nylon 12, 65% Glass Fiber Filled, Conditioned
 39EMS-Grivory Grilamid® LV-65H FWA nat Nylon 12, 65% Glass Fiber Filled, Dry
 40EMS-Grivory Grilamid® LV-65H FWA nat Nylon 12, 65% Glass Fiber Filled, Conditioned
 41EMS-Grivory Grilamid® LV-65H SST black 9288 Nylon 12, 65% Glass Fiber Filled, Dry
 42EMS-Grivory Grilamid® LV-65H SST black 9288 Nylon 12, 65% Glass Fiber Filled, Conditioned
 43EMS-Grivory Grilamid® LV-65H SST nat Nylon 12, 65% Glass Fiber Filled, Dry
 44EMS-Grivory Grilamid® LV-65H SST nat Nylon 12, 65% Glass Fiber Filled, Conditioned
 45EMS-Grivory Grilamid® LVX-50H black 9230 Nylon 12, 50% Glass Fiber Filled, Dry
 46EMS-Grivory Grilamid® LVX-50H black 9230 Nylon 12, 50% Glass Fiber Filled, Conditioned
 47EMS-Grivory Grilamid® LVX-50H nat Nylon 12, 50% Glass Fiber Filled, Dry
 48EMS-Grivory Grilamid® LVX-50H nat Nylon 12, 50% Glass Fiber Filled, Conditioned
 49EMS-Grivory Grilamid® LVX-65H SST black 9288 Nylon 12, 50% Glass Fiber Filled, Dry
 50EMS-Grivory Grilamid® LVX-65H SST black 9288 Nylon 12, 50% Glass Fiber Filled, Conditioned
 
Found 62 Results -- Page of 2 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Instructions: This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database.  Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the 'Find' button next to its box.  You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.


Proto3000 - Rapid Prototyping

Notes:

Top

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.