MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® LBV-65H FWA nat PA12-GF65
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 50% Glass Fiber Filled

Material Notes: Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features:
  • High stiffness combined with good toughness
  • High elongation
  • Very low water absorption
  • Hydrolysis and chemical resistance
  • Easy processing, particularly suitable for thick-walled moldings
The special composition of Grilamid LBV-65H FWA makes it suitable for the direct contact with potable water up to 85°C as well as with foodstuff.

Grilamid LBV-65H FWA natural is designed for applications predominantly in the following application fields:

  • Robust valves and fittings for water and gas supply.
  • Taps, fittings, meters, pumps in sanitary equipment
  • Domestic appliances and household goods
  • Components in the food processing industry

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³Dry; ISO 1183
Water Absorption 0.80 %0.80 %Sim. to ISO 62
Moisture Absorption 0.400 %0.400 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 88
@Time 15.0 sec
88
@Time 0.00417 hour
Conditioned; ISO 868
Ball Indentation Hardness 230 MPa33400 psiConditioned; ISO 2039-1
Tensile Strength at Break 170 MPa24700 psiConditioned; ISO 527-1/-2
 190 MPa27600 psiDry; ISO 527-1/-2
Elongation at Break 3.0 %3.0 %Dry; ISO 527-1/-2
 3.0 %3.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 18.5 GPa2680 ksiConditioned; ISO 527-1/-2
 20.0 GPa2900 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 35.0 kV/mm889 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C41.7 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C194 - 248 °FLong Term; ISO 2578
 160 °C320 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 130 °C266 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
Food contactEU Requirements
FormGranules
Industry & Consumer goodsHeating systems
 Sanitary, water and gas supply
ProcessingInjection Molding
Product AttributesHydrolysis resistant
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)
Water ContactACS
 DVGW W270
 KTW
 NSF 61
 WRAS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE)
Röchling LAMIGAMID® 1200 Cast Polyamide 12, Dry
Momentive Performance Materials Silopren™ LSR 2070 Liquid Silicone Rubber - General Purpose
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE
Klinger Thermoseal KLINGER® top-chem-2000 PTFE Gasketing

PGRH064 / 156773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.