MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Material Category Search

Find a Material Category:
Select a Material Category: Selected Material Category:
  Search Results
There are 55 materials in the category Polyethylene Terephthalate (PET), Glass/Mineral Reinforced. If your material is not listed, please refer to our search strategy page for assistance in limiting your search.

Found 55 Results -- Page of 2 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
 2DiscontinuedCovestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
 3DiscontinuedCovestro Petlon® 8535 Semi-Crystalline PET, 35% Mineral/Glass Fiber
 4DiscontinuedCovestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber
 5DiscontinuedCovestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber
 6DiscontinuedCovestro Petlon® 4835 Semi-Crystalline PET, 35% Mineral/Glass Fiber
 7A. Schulman ComAlloy Comtuf® 462 Glass/Mineral Reinforced, PET Alloy, Impact Modified, UL
 8A. Schulman ComAlloy Hiloy® 446 Glass/Mineral Reinforced, PET Alloy
 9A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL
 10A. Schulman COMTUF® 462 Glass/Fiber Mineral Reinforced, Impact Modified PET Alloy
 11BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET
 12Adell WL-38 40% Glass and Mineral Reinforced PET
 13Celanese Rynite® FR335 BK507 PET, 35% Glass/Mineral Reinforced
 14Celanese Rynite® FR335 NC010 PET-GF35FR(30+16)
 15Celanese Rynite® FR945 BK507 PET-(MD+GF)45FR(17)
 16Celanese Rynite® RE5231 BK533 PET-(GF+MD)35
 17Celanese Rynite® 935 BK505 PET-(MD+GF)35
 18Celanese Rynite® 935 NC010 PET-(MD+GF)35
 19Celanese Rynite® 935SUV BK593 PET-(MD+GF)35
 20Celanese Rynite® 940 BK505 PET-(GF+MD)40
 21Celanese Rynite® 940 NC010 PET-(GF+MD)40
 22Celanese Rynite® 940E BK505 PET-(GF+MD)40
 23Celanese Rynite® RE19051 BK507 Polyethylene Terephthalate (PET)
 24E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET
 25Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
 26Gromax PET 9030-104E 30% Glass/Mineral Filled
 27Celanese Impet® 830R PET, 35% Mineral / Glass Reinforced
 28Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced
 29Lavergne VYPET VNT 335 PET 35% Glass - Mineral Reinforced
 30Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced
 31Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced
 32Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced
 33Lavergne VYPET VNT 840 HY PET 40% Glass-Mineral Reinforced
 34DiscontinuedA. Schulman Matrixx 80M7451 45% Glass/Mineral Filled PET
 35MRC Polymers MAXNITE™ 550 GF30 PET, 30% Glass Mineral Reinforced
 36DiscontinuedCustom Resins Vexel™ E20MG35 , 35% Glass/Mica Reinforced PET
 37Polyplastics FR-PET® BLR6001MZ Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET)
 38Polyplastics FR-PET® C9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
 39Polyplastics FR-PET® B3030FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
 40Polyplastics FR-PET® B3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
 41Polyplastics FR-PET® C3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
 42Polyplastics FR-PET® B3045FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
 43Polyplastics FR-PET® B9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
 44Polyplastics FR-PET® CN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
 45Polyplastics FR-PET® CN9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
 46Polyplastics FR-PET® C3030FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
 47Polyplastics FR-PET® BN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
 48Polyplastics FR-PET® CN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
 49Polyplastics FR-PET® BN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose
 50RTP Company RTP 1104 M 15 BLK Polyethylene Terephthalate (PET), 25% Glass Fiber - 15% Mineral
 
Found 55 Results -- Page of 2 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Instructions: This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database.  Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the 'Find' button next to its box.  You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.


Proto3000 - Rapid Prototyping

Notes:

Top

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.