MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Rynite® 935SUV BK593 PET-(MD+GF)35
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass/Mineral Reinforced

Material Notes: 35% Glass Reinforced, UV Stabilized, Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527-1/-2
Elongation at Break 2.3 %2.3 %ISO 527-1/-2
Tensile Modulus 9.70 GPa1410 ksiISO 527-1/-2
Poissons Ratio 0.340.34
Charpy Impact Unnotched 2.40 J/cm²
@Temperature 23.0 °C
11.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 252 °C486 °F10°C/min; ISO 11357-1/-3
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Glow Wire Test  750 °C
@Thickness 0.750 mm
1380 °F
@Thickness 0.0295 in
No Flame; IEC 60335-1
 750 °C
@Thickness 1.00 mm
1380 °F
@Thickness 0.0394 in
No Flame; IEC 60335-1
 750 °C
@Thickness 1.50 mm
1380 °F
@Thickness 0.0591 in
No Flame; IEC 60335-1
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
No Flame; IEC 60335-1
Glow Wire Ignition Temperature  750 °C
@Thickness 0.400 mm
1380 °F
@Thickness 0.0157 in
IEC 60695-2-12
 750 °C
@Thickness 0.750 mm
1380 °F
@Thickness 0.0295 in
IEC 60695-2-13
 750 °C
@Thickness 1.00 mm
1380 °F
@Thickness 0.0394 in
IEC 60695-2-13
 750 °C
@Thickness 1.50 mm
1380 °F
@Thickness 0.0591 in
IEC 60695-2-13
 875 °C
@Thickness 3.00 mm
1610 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  750 °C
@Thickness 0.400 mm
1380 °F
@Thickness 0.0157 in
IEC 60695-2-12
 750 °C
@Thickness 0.750 mm
1380 °F
@Thickness 0.0295 in
IEC 60695-2-12
 750 °C
@Thickness 1.00 mm
1380 °F
@Thickness 0.0394 in
IEC 60695-2-12
 750 °C
@Thickness 1.50 mm
1380 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 °C545 °FOptimum, Injection
 280 - 300 °C536 - 572 °FRange, Injection
Mold Temperature 110 °C230 °FOptimum, Injection
 100 - 120 °C212 - 248 °FInjection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %<= 0.020 %Injection
Hold Pressure >= 80.0 MPa>= 11600 psiInjection
 
Descriptive Properties
AdditivesRelease agent
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0.1G-value (condensate); ISO 6452
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PET-(MD+GF)35<ISO 11469
PolymerPET-(P+GF)35
Processing Hold Pressure Time (s/mm)4Injection
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPET-(MD+GF)35ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lavergne VYPET VNT 635A PET 35% Glass Reinforced
Celanese Rynite® 408 NC010 PET
Carbon-Core CarbonFoam 100 PET
Aclo Accucomp PET PET008L
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)

PDSX5266 / 197906

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.