MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Rynite® 935SUV BK593 PET-(MD+GF)35
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass/Mineral Reinforced

Material Notes: 35% Glass Reinforced, UV Stabilized, Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527-1/-2
Elongation at Break 2.3 %ISO 527-1/-2
Tensile Modulus 9700 MPaISO 527-1/-2
Poissons Ratio 0.34
Charpy Impact Unnotched 24.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 252 °C10°C/min; ISO 11357-1/-3
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Glow Wire Test 750 °C
@Thickness 0.750 mm
No Flame; IEC 60335-1
 750 °C
@Thickness 1.00 mm
No Flame; IEC 60335-1
 750 °C
@Thickness 1.50 mm
No Flame; IEC 60335-1
 850 °C
@Thickness 3.00 mm
No Flame; IEC 60335-1
Glow Wire Ignition Temperature 750 °C
@Thickness 0.400 mm
IEC 60695-2-12
 750 °C
@Thickness 0.750 mm
IEC 60695-2-13
 750 °C
@Thickness 1.00 mm
IEC 60695-2-13
 750 °C
@Thickness 1.50 mm
IEC 60695-2-13
 875 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 750 °C
@Thickness 0.400 mm
IEC 60695-2-12
 750 °C
@Thickness 0.750 mm
IEC 60695-2-12
 750 °C
@Thickness 1.00 mm
IEC 60695-2-12
 750 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 285 °COptimum, Injection
 280 - 300 °CRange, Injection
Mold Temperature 110 °COptimum, Injection
 100 - 120 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %Injection
Hold Pressure >= 80.0 MPaInjection
 
Descriptive Properties
AdditivesRelease agent
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0.1G-value (condensate); ISO 6452
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PET-(MD+GF)35<ISO 11469
PolymerPET-(P+GF)35
Processing Hold Pressure Time (s/mm)4Injection
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPET-(MD+GF)35ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lavergne VYPET VNT 635A PET 35% Glass Reinforced
Celanese Rynite® 408 NC010 PET
Carbon-Core CarbonFoam 100 PET
Aclo Accucomp PET PET008L
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)

PDSX5266 / 197906

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.