MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 00755 Melamine-Phenolic, Granular, Compression Molded
Categories: Polymer; Thermoset; Melamine; Melamine-Phenolic Copolymer; Phenolic

Material Notes: PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755 is available only in brown.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.580 g/cc0.0210 lb/in³ASTM D1895
Density 1.60 g/cc0.0578 lb/in³ASTM D792
Water Absorption 0.36 %0.36 %ASTM D570
Linear Mold Shrinkage 0.0042 cm/cm0.0042 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7171ASTM D785
Tensile Strength, Ultimate 56.0 MPa8120 psiASTM D638
Elongation at Break 0.64 %0.64 %ASTM D638
Tensile Modulus 10.0 GPa1450 ksiASTM D638
Flexural Strength 89.0 MPa12900 psiASTM D790
Flexural Modulus 8.90 GPa1290 ksiASTM D790
Compressive Strength 165 MPa23900 psiASTM D695
Izod Impact, Notched 0.201 J/cm0.377 ft-lb/inASTM D256
Charpy Impact, Notched 0.221 J/cm²1.05 ft-lb/in²ASTM D256
Impact 148148J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.80e+13 ohm-cm1.80e+13 ohm-cmASTM D247
Dielectric Constant 6.56.5ASTM D150
Dielectric Strength 8.50 kV/mm216 kV/inStep by Step; ASTM D149
 12.0 kV/mm305 kV/inShort Time; ASTM D149
Dissipation Factor 0.0540.054ASTM D150
Arc Resistance 186 sec186 secASTM D495
Comparative Tracking Index 425 V425 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.580 W/m-K
@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 152 °C306 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 184 °C363 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 33 %33 %ASTM D2863
Shrinkage 0.89 %0.89 %240 hr, 105ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Melamine-Phenolic Copolymer
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
Overview of materials for Vinyl Ester Sheet Molding Compound
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
Overview of materials for Epoxy Molding Compound

PLEL07 / 50575

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.