MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AGY ADVANTEX® Generic Glass Fiber
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: OC/AGY E-CR glass. Various silanes and starch oil are used as binders. Acid resistant. Lower alkali resistance than VeTron® and ZenTron® glass fibers.

Information provided by AGY Holding Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.624 g/cc0.09480 lb/in³
Water Absorption 0.00 %0.00 %
Loss On Ignition 0.50 - 1.5 %0.50 - 1.5 %Varies according to size type
Filament Diameter 9.0 - 30 µm9.0 - 30 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  2450 MPa
@Temperature 371 °C
355000 psi
@Temperature 700 °F
 3200 - 3750 MPa
@Temperature 23.0 °C
464000 - 544000 psi
@Temperature 73.4 °F
Elongation at Break 4.5 %4.5 %in 50 mm
Modulus of Elasticity 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.84e+14 ohm-cm3.84e+14 ohm-cm
Dielectric Constant  7.2
@Frequency 1000 Hz
7.2
@Frequency 1000 Hz
 7.5
@Frequency 1e+10 Hz
7.5
@Frequency 1e+10 Hz
Dielectric Strength 10.0 kV/mm254 kV/in
Dissipation Factor 0.00280.0028
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.80 µm/m-°C
@Temperature -30.0 - 300 °C
3.22 µin/in-°F
@Temperature -22.0 - 572 °F
average, isotropic
Specific Heat Capacity 0.970 J/g-°C
@Temperature 200 °C
0.232 BTU/lb-°F
@Temperature 392 °F
Melting Point 1171 °C2140 °FLiquidus
Liquidus 1171 °C2140 °F
Maximum Service Temperature, Air 740 °C1360 °F
Maximum Service Temperature, Inert 740 °C1360 °F
Transformation Temperature, Tg 750 °C1380 °F
Softening Point 916 °C1680 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.561.56

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
E-CRGlas® Fiber
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Park Aerospace Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced
Park Aerospace Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced

CGLASS01 / 931

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.