MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 12, 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.96 g/cc0.0415 - 0.0708 lb/in³Average value: 1.26 g/cc Grade Count:80
Filler Content 25.0 - 30.0 %25.0 - 30.0 %Average value: 28.8 % Grade Count:4
Water Absorption 0.100 - 1.40 %0.100 - 1.40 %Average value: 0.720 % Grade Count:45
Moisture Absorption at Equilibrium 0.400 - 0.600 %0.400 - 0.600 %Average value: 0.531 % Grade Count:27
Water Absorption at Saturation 1.00 - 1.40 %1.00 - 1.40 %Average value: 1.13 % Grade Count:36
Linear Mold Shrinkage 0.00100 - 0.0130 cm/cm0.00100 - 0.0130 in/inAverage value: 0.00427 cm/cm Grade Count:54
Linear Mold Shrinkage, Transverse 0.00100 - 0.0110 cm/cm0.00100 - 0.0110 in/inAverage value: 0.00447 cm/cm Grade Count:38
Melt Flow 7.00 - 23.0 g/10 min7.00 - 23.0 g/10 minAverage value: 12.6 g/10 min Grade Count:7
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109 - 110109 - 110Average value: 110 Grade Count:4
Hardness, Shore D 73.0 - 83.073.0 - 83.0Average value: 80.3 Grade Count:19
Ball Indentation Hardness 120 - 170 MPa17400 - 24700 psiAverage value: 135 MPa Grade Count:15
Tensile Strength, Ultimate 12.0 - 150 MPa1740 - 21800 psiAverage value: 107 MPa Grade Count:54
 35.0 - 95.0 MPa
@Temperature 60.0 - 150 °C
5080 - 13800 psi
@Temperature 140 - 302 °F
Average value: 58.8 MPa Grade Count:2
Tensile Strength, Yield 38.0 - 150 MPa5510 - 21800 psiAverage value: 104 MPa Grade Count:31
Elongation at Break 2.00 - 15.0 %2.00 - 15.0 %Average value: 5.87 % Grade Count:70
 4.50 - 16.0 %
@Temperature 60.0 - 150 °C
4.50 - 16.0 %
@Temperature 140 - 302 °F
Average value: 9.38 % Grade Count:2
Elongation at Yield 3.00 - 50.0 %3.00 - 50.0 %Average value: 8.12 % Grade Count:17
 >= 10.0 %
@Temperature 60.0 - 150 °C
>= 10.0 %
@Temperature 140 - 302 °F
Average value: 10.0 % Grade Count:1
Modulus of Elasticity 1.80 - 15.8 GPa261 - 2290 ksiAverage value: 6.67 GPa Grade Count:68
 2.10 - 7.20 GPa
@Temperature 60.0 - 150 °C
305 - 1040 ksi
@Temperature 140 - 302 °F
Average value: 4.04 GPa Grade Count:2
Flexural Yield Strength 120 - 240 MPa17400 - 34800 psiAverage value: 159 MPa Grade Count:19
Flexural Modulus 3.70 - 11.5 GPa537 - 1670 ksiAverage value: 5.66 GPa Grade Count:22
Izod Impact, Notched 1.07 - 1.80 J/cm2.00 - 3.37 ft-lb/inAverage value: 1.32 J/cm Grade Count:13
Izod Impact, Unnotched 5.34 - 5340 J/cm10.0 - 10000 ft-lb/inAverage value: 7.12 J/cm Grade Count:8
Izod Impact, Notched (ISO) 5.00 - 17.0 kJ/m²2.38 - 8.09 ft-lb/in²Average value: 12.6 kJ/m² Grade Count:5
Charpy Impact Unnotched 1.10 J/cm² - NB5.24 ft-lb/in² - NBAverage value: 8.01 J/cm² Grade Count:53
 2.00 J/cm² - NB
@Temperature -40.0 - -20.0 °C
9.52 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 8.10 J/cm² Grade Count:45
Charpy Impact, Notched 0.650 - 2.80 J/cm²3.09 - 13.3 ft-lb/in²Average value: 1.67 J/cm² Grade Count:55
 0.600 - 2.10 J/cm²
@Temperature -40.0 - -20.0 °C
2.86 - 9.99 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.26 J/cm² Grade Count:47
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.00e+15 ohm-cm100 - 1.00e+15 ohm-cmAverage value: 1.49e+14 ohm-cm Grade Count:44
Surface Resistance 1000 - 1.00e+15 ohm1000 - 1.00e+15 ohmAverage value: 1.14e+14 ohm Grade Count:31
Dielectric Constant 3.00 - 4.903.00 - 4.90Average value: 3.88 Grade Count:11
Dielectric Strength 17.7 - 45.0 kV/mm450 - 1140 kV/inAverage value: 36.3 kV/mm Grade Count:26
Dissipation Factor 0.00420 - 0.07520.00420 - 0.0752Average value: 0.0376 Grade Count:11
Comparative Tracking Index 575 - 600 V575 - 600 VAverage value: 598 V Grade Count:26
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.00 - 80.0 µm/m-°C1.67 - 44.4 µin/in-°FAverage value: 38.5 µm/m-°C Grade Count:33
CTE, linear, Transverse to Flow 50.0 - 150 µm/m-°C27.8 - 83.3 µin/in-°FAverage value: 113 µm/m-°C Grade Count:20
Thermal Conductivity 0.160 - 0.432 W/m-K1.11 - 3.00 BTU-in/hr-ft²-°FAverage value: 0.342 W/m-K Grade Count:3
Melting Point 165 - 185 °C329 - 365 °FAverage value: 177 °C Grade Count:48
Maximum Service Temperature, Air 80.0 - 170 °C176 - 338 °FAverage value: 127 °C Grade Count:24
Deflection Temperature at 0.46 MPa (66 psi) 138 - 182 °C280 - 360 °FAverage value: 172 °C Grade Count:32
Deflection Temperature at 1.8 MPa (264 psi) 90.0 - 177 °C194 - 351 °FAverage value: 157 °C Grade Count:57
Deflection Temperature at 8.0 MPa 65.0 - 125 °C149 - 257 °FAverage value: 93.3 °C Grade Count:18
Vicat Softening Point 165 - 177 °C329 - 351 °FAverage value: 173 °C Grade Count:18
Glass Transition Temp, Tg 40.0 - 45.0 °C104 - 113 °FAverage value: 42.6 °C Grade Count:5
Flammability, UL94 HB - V-0HB - V-0Grade Count:46
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 266 °C338 - 510 °FAverage value: 233 °C Grade Count:5
Melt Temperature 50.0 - 300 °C122 - 572 °FAverage value: 239 °C Grade Count:28
Mold Temperature 40.0 - 104 °C104 - 220 °FAverage value: 75.3 °C Grade Count:28
Injection Velocity 30.0 - 950 mm/sec1.18 - 37.4 in/secAverage value: 348 mm/sec Grade Count:7
Drying Temperature 70.0 - 100 °C158 - 212 °FAverage value: 82.4 °C Grade Count:16
Moisture Content 0.0220 - 0.150 %0.0220 - 0.150 %Average value: 0.113 % Grade Count:9
Injection Pressure 30.0 - 200 MPa4350 - 29000 psiAverage value: 105 MPa Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12
Overview of materials for Nylon 12, Carbon Fiber Filled
Overview of materials for Nylon 12, 20% Glass Fiber Filled
Overview of materials for Nylon 12, 40% Glass Fiber Filled
Overview of materials for Nylon 66, Unreinforced

O2653 / 78074

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.