MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 22-30/AboCure 50-4 Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. AboCast 22-30/AboCure 50-4 is a slow, thick, filled, black, opaque, room-temperature-cure, medium-viscosity epoxy system. It is the preferred system for most casting applications. It offers good thermal conductivity, minimum shrinkage, and low exotherm (heat of reaction). AboCure 50-4 can be mixed in ratios variable from 16 to 50 pbw with 100 pbw AboCast 22-30 for different cured properties: higher rigidity, chemical and heat resistance with the lower AboCure ratios (16-20 pbw), or higher flexibility with higher ratios. The converter offers the lower exotherm that permits unusually heat-sensitive or large castings. The system is used for encapsulation, potting, and assembly of electronic and magnetic components, such as: capacitors, transformers, terminals, industrial magnets, small and large magnetic assemblies, metal detectors, metal separators, magnetic printing cylinders, magnetic holders, insulators, junction boxes, switches, and circuit boards. It is also used in general-purpose casting and bonding for structural and dielectric applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³AboCure 50-4
 1.49 g/cc0.0537 lb/in³AboCast 22-30
Water Absorption 0.19 %
@Time 605000 sec
0.19 %
@Time 168 hour
Viscosity 18600 cP18600 cP
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 92.4 MPa13400 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.10e+15 ohm-cm8.10e+15 ohm-cm"A"
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °FDeflection Temp at unknown load
 
Processing PropertiesMetricEnglishComments
Pot Life 120 - 180 min120 - 180 min
 
Descriptive Properties
ColorBlack
Parts by Weight (pbw)100AboCast 22-30
 25AboCure 50-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboCast 10-5/AboCure 3-4 Epoxy
Overview of materials for Epoxy Cure Resin
Overview of materials for Epoxy, Thermally Conductive
Abatron AboCast 10-5/AboCure 50-12 Epoxy
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy

PABC816 / 107800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.